The low-carbon nitrogen-strengthened chromium nickel stainless steel TP304LN is mainly used in chemical processing, power plants, and heat exchanger systems. Designed for applications requiring enhanced mechanical strength and excellent resistance to intergranular corrosion, this grade maintains superior toughness even at cryogenic temperatures. Furthermore, this grade is suitable for TIG, MAG and manual arc welding procedures.
Single Random, Double Random & Required Length / U Bend
End
Plain End, Beveled End
End Protection
Plastic Caps
Outside Finish
2B, BA, AP, Polished
Delivery Condition
Solution Annealed and Pickled, Bright Annealed, Cold Drawn
Inspection, Test Reports
Mill Test Certificates, EN 10204 3.1, Eddy Current Test, Hydrostatic Test
Packing
Packed in Wooden Boxes, or as per Customers Requests
Specials
Sizes and Specifications other than above can be manufactured on request
TP 304LN . UNS S30453 . 1.4311 Chemical Composition
Chemical Composition (in % by mass)
Grade
C (Max.)
Si (Max.)
Mn (Max.)
P (Max.)
S (Max.)
Cr
Ni
Mo
Ti
N
Others
304LN
0.035
1.00
2.00
0.045
0.030
18.0 - 20.0
8.0 - 11.0
-
-
0.10 - 0.16
-
1.4311
0.030
1.00
2.00
0.045
0.015
17.5 - 19.5
8.5 - 11.5
-
-
0.12 - 0.22
-
TP 304LN . UNS S30453 . 1.4311 Mechanical Property
Mechanical Property & Heat Treatment
Grade
Rp 0.2 Mpa (Min.)
Rp 1.0 Mpa (Min.)
Rm Mpa (Min. - Max.)
A (%) (Min.)
Hardness (HRB) (Max.)
Heat Treatment
304LN
205
-
515
35
90
Solution Annealed
1.4311
270
300
550 - 760
Frequently Asked Questions (FAQ)
What standards and sizes apply to TP304LN / 1.4311 stainless steel tubes?
TP304LN / 1.4311 seamless stainless steel tubes strictly comply with ASME SA213 and ASTM A213 standards. Available outside diameters range from 1/8" OD to 5" OD (6.35 mm to 127 mm) with wall thicknesses from 0.5 mm to 15 mm.
What is the chemical composition difference between 304LN and 1.4311?
Grade 304LN has a maximum carbon content of 0.035% with a nitrogen range of 0.10 - 0.16%. Grade 1.4311 has a slightly lower maximum carbon content of 0.030% and a higher nitrogen content between 0.12 - 0.22%. Chromium and Nickel levels remain similar (Cr: 17.5–20.0%, Ni: 8.0–11.5%).
What are the mechanical property requirements for TP304LN tubes?
TP304LN tubes feature a minimum yield strength (Rp 0.2) of 205 MPa, minimum tensile strength (Rm) of 515 MPa, minimum elongation of 35%, and a maximum hardness of 90 HRB under Solution Annealed condition.
What forms, finishes, and end types are available?
These tubes can be supplied in Round or U Bend forms with Plain or Beveled ends. Available outer surface finishes include 2B, BA (Bright Annealed), AP (Annealed & Pickled), and Polished finishes.
What quality inspection reports are provided with the delivery?
All tube orders come standard with Mill Test Certificates according to EN 10204 3.1. Quality assurance tests include Eddy Current Testing and Hydrostatic Testing.
How are the tubes packaged to prevent damage during transit?
The ends of the tubes are equipped with plastic protective caps. The tubes are packed securely in sturdy wooden boxes or customized according to specific customer requests.