| Grade | C | Si | Mn | P | S | Cr | Ni | Mo | Ti | N | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Max. | Max. | Max. | Max. | Max. | |||||||
| 317L | 0.030 | 1.00 | 2.00 | 0.045 | 0.030 | 18.0 - 20.0 | 11.0 - 15.0 | 3.0 - 4.0 | |||
| 1.4438 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 17.5 - 19.5 | 13.0 - 16.0 | 3.0 - 4.0 | 0.10 |
| Grade | Rp 0.2 | Rp 1.0 | Rm | A (%) | Hardness (HRB) | Heat Treatment |
|---|---|---|---|---|---|---|
| Mpa Min. | Mpa Min. | Mpa Min. - Max. | Min. | Max. | ||
| 317L | 205 | 515 | 35 | 90 | Solution Annealed | |
| 1.4438 | 220 | 250 | 490 - 690 | 35 | Solution Annealed |
| OD (mm) | Thickness (mm) | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 0.50 | 0.70 | 0.80 | 0.89 | 1.00 | 1.20 | 1.24 | 1.50 | 1.65 | 2.00 | 2.11 | 2.50 | 2.77 | 3.05 | |
| 6.00 | x | x | x | x | x | x | x | x | ||||||
| 6.35 | x | x | x | x | x | x | x | x | x | |||||
| 7.00 | x | x | x | x | x | x | x | x | ||||||
| 7.50 | x | x | x | x | x | x | x | x | ||||||
| 8.00 | x | x | x | x | x | x | x | x | ||||||
| 9.00 | x | x | x | x | x | x | x | x | ||||||
| 9.53 | x | x | x | x | x | x | x | x | x | |||||
| 10.00 | x | x | x | x | x | x | x | x | ||||||
| 11.00 | x | x | x | x | x | x | x | x | ||||||
| 12.00 | x | x | x | x | x | x | x | x | x | |||||
| 12.70 | x | x | x | x | x | x | x | x | x | x | x | |||
| 13.00 | x | x | x | x | x | x | x | x | ||||||
| 14.00 | x | x | x | x | x | x | x | x | ||||||
| 15.00 | x | x | x | x | x | x | x | x | ||||||
| 15.88 | x | x | x | x | x | x | x | x | x | x | x | |||
| 16.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 17.15 | x | x | x | x | x | x | x | x | x | x | x | |||
| 18.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 19.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 19.05 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 20.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 21.34 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 22.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 22.23 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 23.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 24.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 25.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 25.40 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.67 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.90 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 28.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 28.58 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 30.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 31.75 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 32.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 33.40 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 35.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 36.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 38.10 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 42.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 44.50 | x | x | x | x | x | x | x | x | x | |||||
| 48.26 | x | x | x | x | x | x | x | |||||||
| 50.80 | x | x | x | x | x | x | x | x | x | x | x | |||
317L and 1.4438 are low-carbon austenitic stainless steel tube grades enhanced with molybdenum (3.0–4.0%), chromium, and nickel. They offer superior corrosion resistance and high creep resistance compared to standard 316L grades.
While both feature a similar molybdenum content (3.0 - 4.0%), grade 1.4438 requires a stricter maximum sulfur content (0.015% max vs 0.030% for 317L), a higher nickel content range (13.0 - 16.0%), and specifies up to 0.10% Nitrogen content.
Grade 317L features a minimum yield strength (Rp 0.2) of 205 MPa, tensile strength (Rm) of min 515 MPa, and max hardness of 90 HRB. Grade 1.4438 provides a minimum yield strength of 220 MPa and tensile strength between 490 - 690 MPa.
Both 317L and 1.4438 stainless steel tubes undergo Solution Annealed heat treatment to maximize corrosion resistance, refine mechanical properties, and remove internal stresses after tube forming.
Common outer diameters (OD) range from 6.00 mm to 50.80 mm, paired with wall thicknesses starting from ultra-thin 0.50 mm up to 3.05 mm, accommodating various industrial pressure and sizing demands.