High-Quality Austenitic steel ASME SA213 · TP304H Manufacturer, Products

The low-carbon chromium nickel stainless steel is mainly used in heat exchangers, boilers, superheaters, and chemical processing. With continuous service temperatures up to 870°C and excellent resistance to intergranular corrosion after welding, this grade shows superior toughness and durability. Furthermore, this grade is suitable for TIG, MAG and manual arc welding procedures.

Product Description

TP304L Stainless Steel Tubes, 1.4307 Stainless Steel Tubes

Item Specification / Details
Stainless Steel Tube ASME SA213, ASTM A213
Tube Size 1/8" OD to 5" OD (6.35 mm to 127 mm)
Thickness Range 0.5 mm – 15 mm
Type Seamless
Form Round, U Bend
Length Single Random, Double Random & Required Length / U Bend
End Plain End, Beveled End
End Protection Plastic Caps
Outside Finish 2B, BA, AP, Polished
Delivery Condition Solution Annealed and Pickled, Bright Annealed, Cold Drawn
Inspection, Test Reports Mill Test Certificates, EN 10204 3.1, Eddy Current Test, Hydrostatic Test
Packing Packed in Wooden Boxes, or as per Customers Requests
Specials Sizes and Specifications other than above can be manufactured on request

TP 304L . UNS S30403 . 1.4307 Chemical Composition

Chemical Composition (in % by mass)
Grade C (Max.) Si (Max.) Mn (Max.) P (Max.) S (Max.) Cr Ni Mo Ti N Others
304L 0.035 1.00 2.00 0.045 0.030 18.0 - 20.0 8.0 - 12.0 - - 0.10 -
1.4307 0.030 1.00 2.00 0.045 0.015 17.5 - 19.5 8.0 - 10.5 - - 0.10 -

TP 304L . UNS S30403 . 1.4307 Mechanical Property

Mechanical Property & Heat Treatment
Grade Rp 0.2 Mpa (Min.) Rp 1.0 Mpa (Min.) Rm Mpa (Min. - Max.) A (%) (Min.) Hardness (HRB) (Max.) Heat Treatment
304L 170 - 485 35 90 Solution Annealed
1.4307 200 230 500 - 700 35 - Solution Annealed

Frequently Asked Questions (FAQ)

Q1 What standard specifications apply to TP304L / 1.4307 stainless steel tubes?

TP304L stainless steel seamless tubes conform to ASME SA213 and ASTM A213 standards. They are available in outer diameters from 1/8" OD to 5" OD (6.35 mm to 127 mm) with wall thicknesses ranging between 0.5 mm and 15 mm.

Q2 What is the chemical composition difference between Grade 304L and EN 1.4307?

Grade 304L contains Chromium between 18.0%–20.0% and Nickel between 8.0%–12.0% with a maximum carbon content of 0.035%. Grade 1.4307 contains Chromium between 17.5%–19.5% and Nickel between 8.0%–10.5% with a maximum carbon content of 0.030%.

Q3 What delivery conditions and surface finishes can be requested?

Tubes can be supplied in Solution Annealed and Pickled, Bright Annealed, or Cold Drawn delivery conditions. Available outside finishes include 2B, BA, AP, and Polished finishes.

Q4 What are the mechanical strength properties of TP304L / 1.4307 tubes?

For Grade 304L, minimum yield strength (Rp 0.2) is 170 MPa, minimum tensile strength (Rm) is 485 MPa, and maximum hardness is 90 HRB. For Grade 1.4307, minimum yield strength (Rp 0.2) is 200 MPa, with tensile strength ranging from 500 to 700 MPa.

Q5 What testing reports and quality controls are provided with the shipment?

Every shipment includes Mill Test Certificates conforming to EN 10204 3.1, along with standard non-destructive testing reports such as Eddy Current Testing and Hydrostatic Testing.

Q6 Are custom tube lengths, forms, or non-standard dimensions available?

Yes, tubes can be ordered in Single Random, Double Random, specified cut lengths, or U-Bend forms. Custom sizes and specifications beyond standard ranges can also be custom manufactured upon request.

Related Products