High-Quality Austenitic steel ASME SA213 · TP347 Manufacturers, Supplier

Tp347 is an austenitic stainless steel stabilized with columbium. The addition of columbium makes this stainless grade perfect performance at high oxidation condition under high temperatures at around 800 degrees Celsius TP347H (UNS S3409) is the stainless steel grade of TP347 with a higher carbon content(0.04 – 0.10) 347H has good resistance to intergranular corrosion, and has good corrosion resistance in alkali, seawater and a variety of acid solutions. Due to its good heat resistance and oxidation resistance, it can withstand small loads at temperatures below 850 degrees.

Product Description

TP347 Stainless Steel Tubes, 1.4550 Stainless Steel Tubes

Item Specification / Details
Stainless Steel Tube ASME SA213, ASTM A213
Tube Size 1/8" OD to 5" OD (6.35 mm to 127 mm)
Thickness Range 0.5 mm – 15 mm
Type Seamless
Form Round, U Bend
Length Single Random, Double Random & Required Length / U Bend
End Plain End, Beveled End
End Protection Plastic Caps
Outside Finish 2B, BA, AP, Polished
Delivery Condition Solution Annealed and Pickled, Bright Annealed, Cold Drawn
Inspection, Test Reports Mill Test Certificates, EN 10204 3.1, Eddy Current Test, Hydrostatic Test
Packing Packed in Wooden Boxes, or as per Customers Requests
Specials Sizes and Specifications other than above can be manufactured on request

TP 347 . UNS S34700 . 1.4550 Chemical Composition

Chemical Composition (in % by mass)

Grade C (Max.) Si (Max.) Mn (Max.) P (Max.) S (Max.) Cr Ni Mo Nb (Cb) N Others
347 0.08 0.75 2.00 0.045 0.030 17.0 - 19.0 9.0 - 13.0 - 10xC - 1.10 - -
1.4550 0.08 1.00 2.00 0.045 0.015 17.0 - 19.0 9.0 - 12.0 - 10xC - 1.00 - -

TP 347 . UNS S34700 . 1.4550 Mechanical Property

Mechanical Property & Heat Treatment

Grade Rp 0.2 Mpa (Min.) Rp 1.0 Mpa (Min.) Rm Mpa (Min. - Max.) A (%) (Min.) Hardness (HRB) (Max.) Heat Treatment
347 205 - 515 35 90 Solution Annealed
1.4550 190 220 500 - 750 30 - Solution Annealed

Frequently Asked Questions (FAQ)

What is TP347 / 1.4550 stainless steel tube?

TP347 (UNS S34700 / 1.4550) is a columbium/niobium-stabilized austenitic stainless steel. The addition of columbium prevents carbide precipitation during heating and welding, making it highly resistant to intergranular corrosion at elevated temperatures.

What are the key advantages of TP347 over standard TP304 tubes?

Compared to TP304, TP347 offers superior creep strength and stress rupture properties at temperatures above 800°F (427°C). Its stabilization with niobium ensures high resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range.

What standards govern ASTM A213 TP347 seamless tubes?

ASTM A213 / ASME SA213 standard covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Material certification generally includes EN 10204 3.1 along with non-destructive testings like Hydrostatic and Eddy Current tests.

What are the typical applications for TP347 / 1.4550 stainless steel tubes?

These tubes are widely used in high-temperature environments such as boiler tubes, superheaters, reheaters, heavy wall fluid piping, petroleum refining equipment, and high-pressure steam service lines.

What delivery conditions and finishes are available?

TP347 seamless tubes are typically supplied in Solution Annealed and Pickled, Bright Annealed (BA), or Cold Drawn conditions. Available surface finishes include 2B, BA, AP, and mechanical polishing according to customer requirements.