High-Quality Austenitic steel ASME SA269 · TP321 Supplier, Products

ASME SA269 TP321 specification is used for general corrosion resisting and high or low temperature service. These tubes have high durability and they can withstand elevated temperatures without losing strength. The SA269 Tubings are cost effective because of their low maintenance and long service life. They are available in heat treated conditions and comes with various finishes.

Product Description

TP321 Stainless Steel Tubing, 1.4541 Stainless Steel Tubing

Item Specification / Details
Stainless Steel Tube ASME SA269, ASTM A269
Tube Size 1/16" OD to 5" OD (1.59 mm to 127 mm)
Thickness Range 0.4 mm – 12.7 mm
Type Seamless & Welded
Form Round, Coiled, Cut-to-Length
Length Single Random, Double Random & Custom Cut Lengths
End Plain End, Beveled End
End Protection Plastic Caps
Outside Finish AP (Annealed & Pickled), BA (Bright Annealed), MP (Mechanical Polished), EP (Electro-polished)
Delivery Condition Solution Annealed and Pickled, Bright Annealed
Inspection, Test Reports Mill Test Certificates, EN 10204 3.1, Flaring Test, Flange Test, Hydrostatic or Nondestructive Electric Test
Packing Packed in Wooden Crates, Plastic Bundles, or as per Customers Requests
Specials Custom sizes and precision instrumentation tubing available upon request

TP 321 . UNS S32100 . 1.4541 Chemical Composition

Chemical Composition (in % by mass)

Grade C (Max.) Si (Max.) Mn (Max.) P (Max.) S (Max.) Cr Ni Mo Ti N (Max.) Others
321 0.08 0.75 2.00 0.040 0.030 17.0 - 19.0 9.0 - 12.0 5x(C+N) - 0.70 0.10
1.4541 0.08 1.00 2.00 0.045 0.015 17.0 - 19.0 9.0 - 12.0 5xC - 0.70 -

TP 321 . UNS S32100 . 1.4541 Mechanical Property

Mechanical Property & Heat Treatment

Grade Rp 0.2 Mpa (Min.) Rp 1.0 Mpa (Min.) Rm Mpa (Min. - Max.) A (%) (Min.) Hardness (HRB) (Max.) Heat Treatment
321 205 515 35 90 Solution Annealed (Min. 1040°C)
1.4541 190 220 500 - 730 30 Solution Annealed

Frequently Asked Questions (FAQ)

What is the difference between TP321 and 1.4541 stainless steel tubing?
TP321 (UNS S32100) is the American standard designation (ASTM/ASME), while 1.4541 (X6CrNiTi18-10) is the European/EN standard designation. Both refer to titanium-stabilized austenitic stainless steel tubing with essentially equivalent chemical compositions and mechanical properties.
Why is Titanium added to TP321 / 1.4541 stainless steel?
Titanium is added to stabilize the steel against chromium carbide formation during exposure to high temperatures (427°C to 816°C). This prevents intergranular corrosion and maintains structural integrity in elevated temperature applications.
What standard specifications apply to TP321 stainless steel tubing?
TP321 stainless steel tubes are commonly manufactured to ASME SA269 and ASTM A269 standards, which cover seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service.
What surface finishes are available for TP321 stainless steel tubing?
TP321 tubing can be supplied in standard finishes including AP (Annealed & Pickled), BA (Bright Annealed), MP (Mechanical Polished), and EP (Electro-polished) based on specific application requirements.
What are the typical applications of TP321 / 1.4541 stainless steel tubes?
Due to high-temperature strength and corrosion resistance, TP321 tubing is widely used in chemical processing, aerospace components, heat exchangers, superheaters, exhaust systems, and high-precision instrumentation.