| Grade | C (Max.) | Si (Max.) | Mn (Max.) | P (Max.) | S (Max.) | Cr | Ni | Mo | Ti | N | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 347 | 0.08 | 1.00 | 2.00 | 0.045 | 0.030 | 17.0 - 19.0 | 9.0 - 12.0 | - | - | - | Nb 10XC - 1.10 |
| 1.4550 | 0.10 | 1.50 | 2.00 | 0.045 | 0.015 | 17.0 - 19.0 | 9.0 - 12.0 | - | - | - | Nb 10XC - 1.10 |
| Grade | Rp 0.2 Mpa (Min.) | Rp 1.0 Mpa (Min.) | Rm Mpa (Min. - Max.) | A (%) (Min.) | Hardness (HRB) (Max.) | Heat Treatment |
|---|---|---|---|---|---|---|
| 347 | 205 | - | 515 | 35 | 90 | Solution Annealed |
| 1.4550 | 205 | 240 | 510 - 740 | 35 | - | Solution Annealed |
| OD | Thickness (mm) | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| (mm) | 0.50 | 0.70 | 0.80 | 0.89 | 1.00 | 1.20 | 1.24 | 1.50 | 1.65 | 2.00 | 2.11 | 2.50 | 2.77 | 3.05 |
| 6.00 | x | x | x | x | x | x | x | x | ||||||
| 6.35 | x | x | x | x | x | x | x | x | x | |||||
| 7.00 | x | x | x | x | x | x | x | x | ||||||
| 7.50 | x | x | x | x | x | x | x | x | ||||||
| 8.00 | x | x | x | x | x | x | x | x | ||||||
| 9.00 | x | x | x | x | x | x | x | x | ||||||
| 9.53 | x | x | x | x | x | x | x | x | x | |||||
| 10.00 | x | x | x | x | x | x | x | x | ||||||
| 11.00 | x | x | x | x | x | x | x | x | ||||||
| 12.00 | x | x | x | x | x | x | x | x | x | |||||
| 12.70 | x | x | x | x | x | x | x | x | x | x | x | |||
| 13.00 | x | x | x | x | x | x | x | x | ||||||
| 14.00 | x | x | x | x | x | x | x | x | ||||||
| 15.00 | x | x | x | x | x | x | x | x | ||||||
| 15.88 | x | x | x | x | x | x | x | x | x | x | x | |||
| 16.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 17.15 | x | x | x | x | x | x | x | x | x | x | x | |||
| 18.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 19.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 19.05 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 20.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 21.34 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 22.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 22.23 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 23.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 24.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | |
| 25.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 25.40 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.67 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 26.90 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 28.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 28.58 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 30.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 31.75 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 32.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 33.40 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 35.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 36.00 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 38.10 | x | x | x | x | x | x | x | x | x | x | x | x | x | x |
| 42.00 | x | x | x | x | x | x | x | x | x | x | ||||
| 44.50 | x | x | x | x | x | x | x | x | x | |||||
| 48.26 | x | x | x | x | x | x | x | |||||||
| 50.80 | x | x | x | x | x | x | x | x | x | x | x | |||
Q1: What is the difference between 347 and 1.4550 stainless steel?
347 is the standard ASTM/AISI grade designation, whereas 1.4550 is the equivalent European EN/DIN standard designation (X6CrNiNb18-10). Both refer to a Niobium-stabilized austenitic stainless steel with nearly identical chemical composition and performance.
Q2: Why is Niobium (Nb) added to Grade 347 / 1.4550 stainless steel?
Niobium is added as a stabilizing element to prevent chromium carbide precipitation during welding and high-temperature exposure (800°F–1500°F / 427°C–816°C), giving it superior resistance to intergranular corrosion.
Q3: What are the main applications for 347 stainless steel tubes?
Common applications include aircraft exhaust stacks, collector rings, boiler casings, chemical processing equipment, radiant superheaters, and heavy-wall welded equipment exposed to high temperatures.
Q4: What heat treatment process is applied to 347 / 1.4550 steel tubes?
They are typically solution annealed at temperature ranges of 1000°C to 1150°C (1832°F to 2102°F), followed by rapid water quenching or air cooling to maintain optimal corrosion resistance and ductility.
Q5: Is Grade 347 stainless steel suitable for welding?